Extruder #2 HIPS material does not stick to previous layer

Description of the problem: HIPS will not stick to the previous HIPS layer

Material: HIPS 1.75mm or 3mm filament

Settings: Support section printed with HIPS as selected in MatterControl Support section. 

Solutions:

  1. Make sure that you have the correct extruder temperature for HIPS - between 230 and 260 C with 100 C on the bed if the support material is printing directly to the bed.
  2. Increase the speed of the support material by going to General>Speed>Speeds for Other Printing and inputting 60 - 80 mm/sec for the Support Material speed.